MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Mg-(11-13)Gd-1Zn ALLOYS

Zhen Rui,Sun Yangshan,Bai Jing,Sun Jingjing,Pi Jinhong
DOI: https://doi.org/10.3724/sp.j.1037.2012.00156
IF: 1.797
2012-01-01
ACTA METALLURGICA SINICA
Abstract:Three ternary alloys with composition of Mg-(11-13)Gd-1Zn (mass fraction, %) have been prepared and their microstructures and mechanical properties have been also investigated. The results showed that the as cast microstructure of the three alloys consists of alpha-Mg matrix, (Mg, Zn)(3)Gd eutectic and a 14H long-period stacking ordered (14H-LPSO) phase. With the increase of Gd content the volume fraction of the (Mg, Zn)(3)Gd eutectic increases. After extrusion the (Mg, Zn)(3)Gd eutectic networks are destroyed and its broken particles are arranged in strips along the direction of extrusion, and the 14H-LPSO phase is distributed between (Mg, Zn)(3)Gd strips. Solid solution treatment at high temperature above 500 degrees C results in the dissolution of (Mg, Zn)(3)Gd phase into the matrix and the increase of the 14H-LPSO phase. After solution treated alloys are aged at temperature of 225 degrees C (T6 treatment) the volume fraction of the 14H-LPSO phase is further increased and both beta' and beta(1) precipitates appear in the microstructure. Aging of as extruded alloys (T5 treatment) also causes the formation of beta' and beta(1) precipitates but the volume fraction of the 14H-LPSO phase in the T5 treated specimens is lower than that in specimens after T6 treatment. High tensile strength combined with good ductility is obtained from the Mg-11Gd-1Zn alloy after T6 aging.
What problem does this paper attempt to address?