Polymer-assisted chemical solution approach to YVO4:Eu nanoparticle networks
qianglu lin,yun xu,engang fu,stacy baber,zongbi bao,liang yu,shuguang deng,janardan kundu,jennifer a hollingsworth,eve bauer,t mark mccleskey,anthony k burrell,quanxi jia,hongmei luo
DOI: https://doi.org/10.1039/c2jm15628h
2012-01-01
Journal of Materials Chemistry
Abstract:Phosphor YVO4:Eu nanoparticle networks were synthesized using water soluble ethylenediaminetetraacetic acid (EDTA) and polyethyleneimine (PEI) as binding ligands. The morphology, particle size, BET surface area, and photoluminescence of YVO4:Eu processed at different annealing temperatures (500, 600, 700, and 800 degrees C) and EDTA/PEI mass ratios (1 : 4, 1 : 2.5, 1 : 2, 1 : 1.5, 1 : 1, 2 : 1, and 4 : 1) were determined by X-ray diffraction, scanning electron microscopy, transmission electron microscopy, fluorescence spectrophotometer, and N-2 adsorption and desorption. The red emission was observed with increasing the annealing temperature. Importantly, the nanoparticles did not aggregate at high annealing temperatures up to 800 degrees C. The smallest size of the YVO4: Eu nanoparticles is about 18 nm and the surface area is 35 m(2) g(-1) with the EDTA/PEI mass ratios of 1 : 1-2.5.