Dynamic Shearing Behavior of Zr_(38)Ti_(17)Cu_(10.5)Co_(12_Be_(22.5) Bulk Metallic Glass

兰山,薛云飞,程焕武,王鲁,张海峰
DOI: https://doi.org/10.3969/j.issn.1004-244x.2009.02.023
2009-01-01
Abstract:The Split Hopkinson Pressure Bar (SHPB) was used to study the failure behavior of Zr-Ti-Cu-Ni bulk metallic glass at room temperature on a strain rate order of 102 s-1. The constitutive behavior of the specimen under dynamic compression is linearly elastic, followed by catastrophic failure with no obviously observed plasticity. The specimen fractured along a dominant shear plane inclined 42° with respect to the loading axis with rough fracture surface. Scanning election microscope (SEM) was used to evaluate the shear banding initiation and propagation. The multiple micro shear bands and mircocracks observed at high magnification on the fracture surface suggest that the dynamic loading promotes crack nucleation immediately following shear banding initiation. Additionally, the observed numerous melted belts on the fracture surface demonstrate that the adiabatic heating plays a significant part on fracture behavior of the Zr-based bulk metallic glass.
What problem does this paper attempt to address?