Synthesis and Characterization of New Aba Triblock Copolymers with Poly[3(S)-Isobutylmorpholine-2,5-Dione] and Poly(Ethylene Oxide) Blocks

YK Feng,D Klee,H Hocker
DOI: https://doi.org/10.1002/(sici)1521-3935(19991001)200:10<2276::aid-macp2276>3.0.co;2-n
IF: 2.996
1999-01-01
Macromolecular Chemistry and Physics
Abstract:ABA type block copolymers with poly[3(S)-isobutylmorpholine-2,5-dione] (PIBMD, A) and poly(ethylene oxide) ((M) over bar(n) = 6000, PEO, B) blocks, PIBMD-b-PEO-b-PIBMD, were synthesized via ring-opening polymerization of 3(S)-isobutylmorpholine-2,5-dione in the presence of hydroxytelechelic poly(ethylene oxide) with stannous octoate as a catalyst. (M) over bar(n) of the resulting copolymers increases with increasing 3(S)-isobutylmorpholine-2,5-dione content in the feed at constant mole ratio of monomer (M) to catalyst (C) (M/C = 125). No racemization of the leucine residue takes place during both homopolymerization of IBMD and polymerization of IBMD in the presence of PEO and Sn(Oct)(2). The melting temperature of the PIBMD segments in the block copolymers depends on the length of the PIBMD blocks. The melting temperature of the PEO blocks is lower than that of the; homopolymer, and the crystallinity of the PEO block decreases with increasing length of the PIBMD blocks. The PIBMD block crystallizes first upon cooling from the melt. This leads to only imperfect crystallization or no crystallization of the PEO blocks.
What problem does this paper attempt to address?