In Vitro Behavior of Fluoridated Hydroxyapatite Coatings in Organic-Containing Simulated Body Fluid

Yongsheng Wang,Sam Zhang,Xianting Zeng,Kui Cheng,Min Qian,Wenjian Weng
DOI: https://doi.org/10.1016/j.msec.2006.03.012
2006-01-01
Materials Science and Engineering C
Abstract:A dense and pure hydroxyapatite [HA, Ca-10(PO4)(6)(OH)(2)] coating and a fluoridated HA [Cal(10)(PO4)(6)(OH)(0.67)F-1.33] are deposited on Ti6Al4V substrates by sol-gel dip coating method. Glucose and bovine serum albumin have been added in standard simulated body fluid (SBF) to form organic-containing SBF in simulation of the physiological blood plasma. The HA and the fluoridated HA coatings are immersed in the standard and modified SBF for time periods of 2, 4, 7, 14 and 28 days at 37 +/- 0.1 degrees C. After soaking, the coating surface is examined for nucleation and growth of apatite using SEM morphological observation. The post-soaking SBF solutions are analyzed via hiductively Coupled Plasma spectroscopy for calcium ion concentration. The results show that at concentration of 40 g/L, bovine serum albumin has significant retardation effect on apatite precipitation from SBF onto pure or fluoridated HA coatings; Fluorine-incorporation in HA has positive bio-activation effect in both standard SBF and organic-containing SBF. However, glucose addition in SBF does not generate significant influence on the bioactivity of HA and fluoridated HA. (c) 2006 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?