Joining of zirconia to zirconia using AgCuTi filler metal

H.Q. Hao,Y.L. Wang,Z.H. Jin,X.T. Wang
DOI: https://doi.org/10.1016/0924-0136(94)01611-4
IF: 6.3
1995-01-01
Journal of Materials Processing Technology
Abstract:The active brazing of partially stabilized ZrO2 to ZrO2 was carried out using Ag57Cu38Ti5 filler metal in a vacuum of 7 × 10−3 Pa. The effects of joining conditions such as temperature (from 1073 to 1323 K) and holding time (from 0 to 60 min) on the joint strength and the interfacial reaction were investigated. The joint strength was evaluated by shear testing. It was shown that the brazing temperature and holding time had a strong influence on the joint strength, which latter was controlled mainly by the interfacial morphologies. A lower or higher temperature and a shorter or a longer holding time were disadvantageous to joint strength due to the thinner reaction layer or cracks present at the interface, the maximum joint strength being acheived at 1123 K for 30 min when the interface reaction layer thickness was about 4.4 μm. X-ray diffraction analyses revealed that the reaction products at the interface between zirconia and filler metal were δ TiO and γ-Agti3, and a layer transition structure with a ZrO2/δ TiO/° TiO + γ AgTi3/γ AgTi3/Ag Cu formed at the interface.
What problem does this paper attempt to address?