The improvement in fatigue life of pure polycrystalline nickel by nitrogen ion implantation

M. H. Xu,S. Patu,Z. G. Wang
DOI: https://doi.org/10.1002/pssa.2211050213
1988-01-01
Abstract:A dose of 2 × 1017 ions/cm2 of nitrogen at 150 keV is implanted into pure polycrystalline nickel. The specimens with and without nitrogen ion implantation are tested in tension-zero fatigue. A 21% increase in endurance limit is found with implantation. The fatigued surfaces are examined by SEM. A lower rate and intensity of slip bands in implanted materials are found. Slip band cracking which is found in the unimplanted specimens is replaced by grain boundary cracking in the implanted specimens. The concentration profile of nitrogen is investigated with AES. Eine Dosis von 2 × 1017 Stickstoff-Ionen/cm2 bei 150 keV wird in reines polykristallines Nickel implantiert. Proben mit und ohne Stickstoffionenimplantation werden im Zugbelastungsermüdungsversuch untersucht. Es wird ein 21%iges Anwachsen der Ausdauergrenze mit Implantation gefunden. Die ermüdeten Oberflächen werden mittels SEM untersucht. Es wird eine geringere Rate und Intensität der Gleitbänder in den implantierten Materialien gefunden. Gleitband-Rißbildung, die in nichtimplantierten Proben auftritt, wird durch Korngrenzenrißbildung in implantierten Proben ersetzt. Das Konzentrationsprofil von Stickstoff wird mittels AES untersucht.
What problem does this paper attempt to address?