Preparation and Sintering of CaO-B2O3-SiO2 System for LTCC Substrate Materials

LONG Chengyi,ZHANG Shuren,ZHOU Xiaohua,LI Bo
DOI: https://doi.org/10.3969/j.issn.1001-2028.2011.07.008
2011-01-01
Abstract:CaO-B2O3-SiO2(CBS) system LTCC material was synthesized by using the mixtrue of CaO-B2O3-SiO2(CBS) glass powder(A powder) prepared through high temperature melting method and CaO-B2O3-SiO2-Al2O3 powder(B powder) prepared through solid-phase method with the mass ratio of 7:3.The effects of sintering temperature on the properties of prepared LTCC materials were investigated.Results show that CBS system LTCC materials sintered at 850 ℃ show good denstified properties:shrinkage at x-y direction is 15.16%,bulk density ρ=2.642 g/cm3,er= 5.99(1 MHz),tanδ3.93×10-4(1 MHz) and bending strength σ = 165 MPa.The prepared LTCC materials can be used as substrate materials.
What problem does this paper attempt to address?