An approach to carbon nanotubes with high surface area and large pore volume

Jun Jie Niu,Jian Nong Wang,Ying Jiang,Lian Feng Su,Jie Ma
DOI: https://doi.org/10.1016/j.micromeso.2006.10.009
IF: 5.876
2007-01-01
Microporous and Mesoporous Materials
Abstract:Multi-walled carbon nanotubes (MWCNTs) with high purity were synthesized by a floating catalyst technique suitable for large-scale production. Ethanol and ferrocene were used as the carbon and catalyst precursors, respectively. Thiophene was added to assist the growth. The pristine sample was chemically activated by using KOH at high temperature and the specific surface area increased drastically from ∼65m2/g to ∼830m2/g while the graphite structure was maintained. Furthermore, the mean pore diameter was decreased from 21.15nm to 7.68nm and pore volume increased from 0.3429cm3/g to 1.5950cm3/g. MWCNTs with a high surface area and pore volume would have promising applications in many fields.
What problem does this paper attempt to address?