Production Process Research and Quality Analysis of 77B Wire Rod

张春燕,冯运莉,张晓光,陈兴伟,李毅平
DOI: https://doi.org/10.3969/j.issn.1003-4226.2010.03.014
2010-01-01
Abstract:To introduce production process of 77B wire rod.Catch carbon practice was carried out while adopting converter smelting.Low basicity about 2.0 to dilute thin sediment when LF furnace was refining,to carry out molten steel narrow ingredient control,whole course protecting casting while continuous casting,to stabilize continuous casting velocity(from 1.7 to 2.3 m /min)by adopting secondary cooling water principle,to control fluctuating scope within ± 0.1 m /min,low superheat casting from 1 000 ℃ to 1 050 ℃,low temperature rolling from 980 ℃ to 1 020 ℃,wire rod laying temperature controlled from 850 ℃ to 870 ℃,roller initial speed 0.8 m /s.Tensile strength of diameter 8.0 mm 77B wire rod produced by Tangsteel is from 1 605 MPa to 1 660 MPa,percentage of elongation is from 4% to 5%,area reduction is from 32% to 38%,product can satisfy using requirement of customers.
What problem does this paper attempt to address?