Surface Grafting of Acrylic Acid/Acrylic Amide onto Fluoroelastomer

Chen Chen,Yong Liu,Dong Wang,Wei Tong,Xinxing Zhang,Canhui Lu
DOI: https://doi.org/10.16865/j.cnki.1000-7555.2011.06.016
2011-01-01
Abstract:The surface of fluoroelastomer was treated by atmospheric pressure dielectric barrier discharge(DBD) in air.Acrylic acid(AA) and acrylic amide(AAm) monomer were further grafted onto the activated fluoroelastomer surface to improve its wettability.The wettability of fluoroelastomer was investigated by water contact angle measurement.The results indicate that the minimum water contact angle(40°) is obtained at grafting time of 60 min and temperature of 60℃for AA-grafting;on the other hand,the minimum water contact angle(51°) is obtained at grafting time of 150 min and temperature of 50℃for AAm-grafting.