Hysteresis Behavior In Raman Intensities In Yba2cu3o7-Y-Family Superconductors Between Tc And T0=234-K

Ming-Sheng Zhang,Qiang Chen,Gongjian Hu,J. F. Scott
DOI: https://doi.org/10.1080/01411599008207221
1990-01-01
Phase Transitions
Abstract:Abstract The intensity of the 646 cm-1 Raman line in YBa2Cu3-x V x O7-y has been measured for cooling and heating from 77 K to 234 K. The intensity exhibits intensity hysteresis of order 20% in the cooling versus heating values between T c = 89 K and T o = 234 K. This effect is unexplained but is extremely similar to that reported by Ledbetter et al. for the bulk modulus and C 11 elastic coefficient. In each case the hysteresis vanishes below T c , independent of the value of T c , which may be adjusted from 60 K to 94 K by changing oxygen concentration y. Qualitative interpretation requires that the structural phase transition near 234 K be intimately related to the superconducting transition at T c presumably through partial ordering of oxygens.