Effects of defibration process on the properties of old corrugated container fiber

GUO Wen-jie,GUAN Ze-yu,WANG Yan,WAN Jin-quan,MA Yong-wen
DOI: https://doi.org/10.3969/j.issn.1007-9211.2010.22.005
2010-01-01
Abstract:Physical and chemical properties and variation in paper properties of old corrugated container (OCC) fiber during defibration process were investigated. The results show that with the increase of defibrating time, the fiber bundles decrease gradually, and became single fiber finally; meanwhile some fibers are cut off on some extent. The average length decreases by 4.35%; but the fines content in- creases by 8.5%, and the water retention value (WRV) of the fibers increases gradually, with the maximum up to 14.3%; the tear and tensile index of the fibers increase by 12% and 22.2% respectively. Defibrating process has little impact on the crystalline degree in the fibres, and no new chemical group appears, but the strength of the hydrogen bonds in cellulose molecules decreases.
What problem does this paper attempt to address?