Deactivation of Catalyst for Hydrogenation of 3-Hydroxypropionaldehyde to 1,3-Propanediol

Tang Yong,Shen Benxian,Ning Chunli,Zhu Xiaodong,Ma Jianxue,Zhang Chunlei
DOI: https://doi.org/10.3321/j.issn:1000-8144.2009.09.007
2009-01-01
Abstract:Ni-M/HM bimetal supported catalyst was used as first-stage hydrogenation catalyst in two stage hydrogenation of 3-hydroxypropionaldehyde(3-HPA) to 1,3-propanediol.Stability of Ni-M/HM catalyst was investigated in a fixed-bed reactor.Deactivation of the catalyst was studied by means of XRD,BET,TG-DTA,ICP-AES,XRF and element analysis.Under reaction conditions:5.0 MPa, LHSV of 3-HPA 2.0 h~(-1),mole ratio of H_2 to 3-HPA 8.0 and reaction temperature 50.0 - 72.0℃,the catalyst deactivated after 3 300 h on-stream time.Framework structure of HM in deactivated catalyst remained.Specific surface area and pore volume of the deactivated catalyst changed apparently,coke formed on the surface of the deactivated catalyst,and loss of Ni from surface of catalyst was determined.The main reason of the deactivation is deposition of oligomers and the secondary reason is loss of superficial Ni species.The activity of deactivated catalyst can be basically recovered after regeneration to the level of fresh catalyst.
What problem does this paper attempt to address?