Foamed ethylene-propylene-diene rubber/polypropylene thermoplastic vulcanizate prepared by chemical foaming Ⅰ. Extrusion processing parameters

Chen Wenquan,Wu Shemao,Tian Hongchi,Zhang Liqun
DOI: https://doi.org/10.3969/j.issn.1000-1255.2008.05.014
2007-01-01
Abstract:The foamed ethylene-propylene-diene rubber/polypropylene thermoplastic vulcanizate(EPDM/PP TPV)was prepared by single screw extruder using azodicarbonamide as chemical blowing agent.The effects of extrusion temperature,head temperature and screw rotation speed on properties and cell morphology of foamed TPV were explored.The results showed that under the premise of ensuring complete plasticization and melting of TPV as well as smooth extrusion,lower extrusion temperature and extruder head temperature was of benefit to the preparation of foamed TPV with low density,fine and uniform cell or high surface quality.The optimal extrusion temperature and head temperature was 185 ℃ and 170 ℃ respectively.With the increase of screw rotation speeds,density and tensile properties of foamed TPV reduced first but then increased,average cell diameter kept constant,cell area density increased first but then decreased,and cell size distribution narrowed first but then broadened.The optimal screw rotation speed was 65 r/min.
What problem does this paper attempt to address?