Fabrication and Compression Properties of Ti Honeycomb

Wang Hongwei,Li Qingfen,Zhu Zhaojun,Wei Zunjie
DOI: https://doi.org/10.3969/j.issn.1007-2330.2007.04.013
2007-01-01
Abstract:Ti metal honeycomb structure materials are fabricated by using Fused Deposition Modelling rapid prototype manufacturing.The techniques of fabricating powder slurry,solidifying Ti metal honeycomb wax and dewaxing cast wax are investigated.Also,the compression properties of fabricated Ti metal honeycomb are studied.The results indicate that Ti metal honeycomb structure can be fabricated by using Fused Deposition Modelling technique and the processes are simple and the size of honeycomb is controllable.When the relative density of Ti honeycomb structure is between 9% and 12.6%,the yield strength and elastic modulus of Ti honeycomb structure have a few increasing.When the relative density of Ti honeycomb structure is over 12.6%, the yield strength of Ti honeycomb structures increases significantly,however, the elastic modulus of Ti honeycomb structure has a little increase.Furthermore,by changing edge length or wall thickness of hexagon,the same relative density of Ti honeycomb structure can be obtained.On the condition of the same relative density by changing edge length and wall thickness of hexagon,the yield strength of Ti honeycomb structure is similar,but the elastic modulus has significant difference.
What problem does this paper attempt to address?