Hydrometallurgical process for recovery of antimony from arsenic-alkali residue

Wang Jianqiang,Wang Yunyan,Wang Xin,Chai Liyuan
DOI: https://doi.org/10.3969/j.issn.1673-9108.2006.01.015
2006-01-01
Abstract:Arsenic-alkali residue is leached by water firstly in order to separate the arsenic and antimony,and then the liquid leached residue is leached by hydrochloric acid,this solution containing SbCl_3 is very useful in industry.Under the optimum conditions such as ratio of liquid to solid being 6,leaching temperature being 40℃ and lasting time being 40 min,the leaching rate of arsenic is above 99% and leaching rate of antimony is blow 3%.During the progress of hydrochloric leaching,controlling the acid concentration being 1∶1,ratio of liquid of solid being 10∶1,temperature being 60℃ and time for 30 min,the leaching rate of antimony exceeds 88%.After the 2 procress of leaching,the direct recovery rate of antimony is 85.36%.