Application of response surface methodology for roasting optimization in composite roasting—Acid leaching vanadium extraction process
Xin Wang,Junyi Xiang,Guishang Pei,Lanjie Li,Qingyun Huang,Xuewei Lv
DOI: https://doi.org/10.1016/j.cherd.2021.06.017
IF: 4.119
2021-08-01
Chemical Engineering Research and Design
Abstract:The effective and environmentally friendly composite roasting with CaO/MgO was applied.The central composite design (CCD) and response surface method (RSM) were applied to optimize the roasting parameters in vanadium extraction process.The leaching efficiency of vanadium, phosphorus and manganese were evaluated.Composite roasting with CaO/MgO and leaching process is an environmentally friendly and simple technique in the treatment of vanadium slag which has been practiced using CaO and MgO as composite roasting additives. The recovery of vanadium is significantly influenced by the roasting parameters, viz., CaO/V<sub>2</sub>O<sub>5</sub> mole ratio (<em>x<sub>1</sub></em>), MgO/V<sub>2</sub>O<sub>5</sub> mole ratio (<em>x<sub>2</sub></em>), roasting temperature (<em>x<sub>3</sub></em>), and holding time (<em>x<sub>4</sub></em>). Therefore, the response surface method (RSM) and central composite design (CCD) were performed to model and optimize the roasting factors in this research. The results shown that the models for the dissolution of vanadium, phosphorus, and manganese show good concordance with the experimental data. Additionally, a multiple response simultaneous optimization using the desirability function was used to find the optimum roasting conditions for the leaching efficiency of vanadium, phosphorus, and manganese. The optimal results were obtained at <em>x<sub>1</sub></em> = 0.84, <em>x<sub>2</sub></em> = 0.40, <em>x<sub>3</sub></em> = 900 °C, and <em>x<sub>4</sub></em> = 1.89 h. Under these conditions, 90.87% vanadium, 13.64% phosphorus, and 48.61% manganese were leached, which were beneficial not only to the recovery of vanadium but also to the minimization of impurity element of phosphorus and the maximum recovery of manganese.<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S0263876221002604-fx1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (115KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S0263876221002604-fx1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
engineering, chemical