Influences of Frequency Ratio of Pulse Power on MAO Coatings on AZ91D Magnesium Alloy

郑俊军,曹发和,冷文华,常林荣,张鉴清
2012-01-01
Abstract:AZ91D magnesium alloy was anodized in alkaline silicate solution using a micro-arc oxidation (MAO) pulse power source under different frequency ratio (FR), which is the ratio of the positive frequency to the negative frequency. The FR changes the distribution of energy density during the MAO process, and then remarkably influences the thickness, morphology and uniformity of the MAO coating. Uniform and thick coating was obtained at FR: 1, and then becomes more porous and thinner with increasing FR due to longer cathodic process in one negative half cycle. The decrease of the interval between two positive pulses with increasing FR results in more discharge channels and more micro-pores on the MAO coating. Many craterlets were formed on the MAO coating because of the dissolution of oxide caused by the lengthened negative half- cycle. Increasing FR, the inner structure of the MAO coating is not obviouslychanged, hence the protectiveness of the anodic coating is not seriously influenced, but the corossion resistance is improved by FR,.
What problem does this paper attempt to address?