The influence of cooling rate on microstructure and magnetic properties of cast Fe-6.5wt%Si steel
J Zhang,K Liu,F Sun,R Liu,G Wu,M Wang,S Gu,Z Zhu,X Mao
DOI: https://doi.org/10.1088/1742-6596/2635/1/012026
2023-11-25
Journal of Physics Conference Series
Abstract:Fe-6.5wt%Si steel samples of different thicknesses (1 mm, 2 mm, and 5 mm) were prepared by arc-melting and suction-casting with sub-rapid solidification rates. The microstructures and magnetic properties of the samples were studied, and the effect of solidification rates were discussed. Results show that columnar crystals are generated with a fiber texture after casting. Ordered phases B2 and D0 3 are inhibited by sub-rapid solidification, and such an effect is clear in the 1 mm thick sample with the largest cooling rate. With decreasing cooling rate, the grain size increases, with the mean values being 66.6±30.8 μm, 93.0±42.8 μm, and 149.7±66.8 μm, and the intensity of the texture increases, with the values being 3.14 mrd, 3.56 mrd, and 5.85 mrd, respectively. The 5 mm thick sample with the lowest cooling rate exhibits the best magnetic properties (B 8 =1.30 T, B 50 =1.55 T, P 1/50 =2.19 W/kg, P 1/400 =37.85 W/kg).