Crystal plasticity modeling of low-cycle fatigue behavior of an Mg-3Al-1Zn alloy based on a model, including twinning and detwinning mechanisms

Xiaoqian Guo,Yao Cheng,Yunchang Xin,Wei Wu,Chao Ma,Ke An,Peter K. Liaw,Peidong Wu,Qing Liu
DOI: https://doi.org/10.1016/j.jmps.2022.105030
IF: 5.582
2022-11-01
Journal of the Mechanics and Physics of Solids
Abstract:The low-cycle fatigue of strongly-textured Mg alloys is dominated mainly by an alternation of twinning-detwinning process, which poses a great challenge to conventional constitutive models. As a result, a good reproduction of both mechanical response and deformation behavior often fails in previous simulations, in particular for high strain amplitudes. In the present study, the numerical simulations of low-cycle fatigue behavior of an Mg AZ31 plate with a ± 2% axial strain amplitude along the rolling direction were conducted, using a modified crystal-plasticity based on the finite strain elastic-viscoplastic self-consistent model containing twinning and detwinning mechanisms (EVPSC-TDT), and the results were compared with the mechanical response and deformation behavior determined by a real-time in-situ neutron diffraction. The simulations well predict the hysteresis loops and cyclic-hardening responses throughout the whole fatigue life (80 cycles), along with the evolution of the maximum twin volume fraction and residual twins. For the first time, the evolution of lattice strain throughout the whole fatigue life was calculated, and the results are in good accordance with that determined by neutron diffraction. The present study strongly demonstrates that the EVPSC-TDT model is very effective for modeling the low-cycle fatigue behavior of Mg alloys. More details about the evolution of the maximum twin volume fraction with fatigue cycles are found, an increase from 1st to 2nd cycle, followed by a decrease from 2nd to 20th cycle and a secondary increase after 20th cycle. This finding corrects the previous opinion that the maximum twin volume fraction increases at the initial stage and tends to be saturated at the late stage. Combining the results of simulations and neutron diffractions, the corresponding reasons are explained. Afterward, the mechanisms of the cyclic-hardening behavior at tension stage and compression stage are revisited, and some new insights are provided.
mechanics,materials science, multidisciplinary,physics, condensed matter
What problem does this paper attempt to address?
The problem that this paper attempts to solve is the modeling of the complex deformation mechanisms in the low - cycle fatigue (LCF) behavior of magnesium alloys (Mg alloys). Specifically, the paper focuses on the low - cycle fatigue behavior of Mg - 3Al - 1Zn alloy (Mg AZ31) with strong texture characteristics under ±2% axial strain amplitude, which is mainly alternately dominated by the twinning - detwinning process. Traditional constitutive models are difficult to accurately simulate the mechanical response and deformation behavior of materials in this process, especially under high strain amplitudes. Therefore, the researchers developed an improved crystal plasticity model based on the finite strain elastic - viscoplastic self - consistent model (EVPSC), which includes twinning and detwinning mechanisms (EVPSC - TDT), in order to better predict the low - cycle fatigue behavior of magnesium alloys. The paper verified the effectiveness of the EVPSC - TDT model through numerical simulation and comparison with the actual neutron diffraction experimental results. The research not only successfully predicted the hysteresis loops and cyclic hardening responses during the entire fatigue life, but also calculated for the first time the lattice strain evolution during the entire fatigue life, and these results are highly consistent with those determined by neutron diffraction. In addition, the study also explored the variation law of the maximum twinning volume fraction with fatigue cycles, and found that it increases in the initial stage, then decreases, and then increases again after 20 cycles, which corrects the previous view that the maximum twinning volume fraction increases in the early stage and tends to saturate in the later stage. Finally, combined with the simulation results and neutron diffraction data, the cyclic hardening mechanisms in the tensile and compressive stages were re - examined, providing new insights.