Pyrolysis of Polyimide Membranes from the Same Dianhydride Monomer and Different Diamines to Form Carbon Membranes
Li Lin,Qi Wen-bo,Wang Hong,Zhang Ping-ping,Sun Mei-yue,Wang Tong-hua,Li Jian-xin,Cao Yi-ming
DOI: https://doi.org/10.1016/j.carbon.2015.10.036
IF: 10.9
2015-01-01
Carbon
Abstract:Polyimide membranes were synthesized by the polymerization of five diamines, p-phenylenediamine (PPD), 2,3,5,6-tetramethyl-1,4-phenylenediamine (TMPPD), 4,4'-oxydianiline (ODA), 4,4'-(4,4'-isopropylidenediphenyl-1,1'-diyldioxy) dianiline (BAPP) and 4,4'-(hexafluoroisopropylidene) bis(p-phenyleneoxy) dianiline (BDAF), and the same dianhydride monomer, 1,2,4,5-benzenetetracarboxylic anhydride (PMDA). The chemical structures of the membranes pyrolyzed at different temperatures were investigated by TGA, TG-MS, FT-IR and XPS. Results indicate that there are five stages during pyrolysis (a) the removal of the solvents, adsorbed oxygen and water, (b) imidization, (c) cross-linking and carbonization, which are accompanied by main chain breaking, (d) deoxygenation and dehydrogenation, (e) aromatization and turbostratic carbon formation: The chemical structure of the precursor is the main factor that causes the great differences in chemical structures during pyrolysis. Imidization in the pyrolysis of the PPD-PMDA and TMPPD-PMDA occurs at higher temperatures than those for ODA-PMDA, BDAF-PMDA and BAPP-PMDA. The order of temperatures for the release of CH4, CO, and C6H6 during the pyrolysis is ODA-PMDA>BDAF-PMDA>BAPP-PMDA. Elemental F in the BDAF-PMDA disappears after pyrolysis at 700 degrees C. The chemical structures of the polyimides have a great influence on the microstructures of the carbon membranes obtained.