Fracture strength of cad-cam milled polyetheretherketone (PEEK) post-cores vs conventional post-cores; an in vitro study

Ayetullah Direk,Samet Tekin,Zohaib Khurshid
DOI: https://doi.org/10.7717/peerj.18012
IF: 3.061
2024-09-05
PeerJ
Abstract:Background: The aim of this study was to compare the fracture strength and fracture modes of post-cores produced with CAD-CAM from modified polyetheretherketone (PEEK) materials with other custom-produced post-cores. Methods: Sixty human mandibular first premolars with equal root sizes were used. The teeth were divided into six groups (n = 10), and root canal treatment was performed. The teeth were separated from the roots over 2 mm from the cemento-enamel junction. As a result of the decoronation process, a 1 mm wide shoulder line was obtained for all teeth. For the fracture strength test, 10 mm deep post spaces were created on the teeth with a 1.6 mm diameter driller. Post-core groups consisted: everStick® glass fiber post-core (Group GF), zirconia post-core (Group Z), metal (Cr-Co) post-core (Group M), PEEK post-core without filler (Group UP), PEEK post-core with 20% TiO2 Filler (Group TP), and post-core with 20% ceramic filler (Group CP). Following the application of posts to post spaces, copings were created and cemented on the samples. With the universal tester, a force was applied to the long axis of the tooth with a slope of 135°. The mean fracture strength (N) between the groups was statistically evaluated using one-way ANOVA, and pairwise mean differences were detected using post hoc Tukey's HSD test among the groups. Results: According to the results of the statistical analysis, a significant difference was found between the groups in terms of mean fracture resistance (p < 0.05). Group Z (409.34 ± 45.72) was significantly higher than Group UP (286.64 ± 37.79), CP (298.00 ± 72.30), and TP (280.08 ± 67.83). Group M (376.17 ± 73.28) was significantly higher than Group UP (286.64 ± 37.79) and Group TP (280.08 ± 67.83). There were no statistically significant differences between the means of the other groups (p > 0.05). Among all the groups, Group Z exhibited a higher prevalence of repairable failure modes, while the rest of the groups predominantly experienced irreparable failure modes. Conclusion: In our study, zirconia and metal post-core samples showed higher average fracture strength values than PEEK post-cores groups. Repairable failure modes were more common in the zirconia post-cores, whereas the opposite was observed in the other groups. Further experimental and clinical trial studies are needed before PEEK materials can be used as post materials in the clinic.
What problem does this paper attempt to address?