High-temperature ball milling: An efficient method to fabricate Ti and its alloy powder for additive manufacturing

Dongdong Chen,Bowen Liu,Guyu Sun,Wei Xu,Yanliang Zhu,Yang An,Langping Zhu,Xianfei Ding,Jiazhen Zhang,Xin Lu
DOI: https://doi.org/10.1016/j.apt.2024.104377
IF: 4.969
2024-03-01
Advanced Powder Technology
Abstract:The low cost effectiveness of spherical titanium and its alloys powder for additive manufacturing (AM) has been widely concerned. This study proposed high-temperature ball milling (HTBM) to modify irregular titanium and its alloys powder for AM, such as hydrogenation-dehydrogenated titanium (HDH Ti), and the ball milling mechanism was revealed. The results showed the irregular HDH Ti powder gradually turning into nearly spherical and flake structures. The modified Ti powder flowability exhibited a mass flow rate of 46.1 ± 0.3 s/50 g, an angle of repose (AOR) of 35.5 ± 0.5° and an oxygen increment of only 300 ppm with a BM T of 490 ℃, a BM t of 14.1 h and a B/M ratio of 2:1, which met the AM requirements. There were continuous fish scale-shaped single and multiple tracks, and complex demonstrative parts were successfully manufactured via selective laser melting using modified powder. The theoretical analysis of the normalized average deformation (Ф) revealed that the modified powder for AM needed meet two requirements: (1) Ф was over 16.7 % and less than 51.5 %, and (2) the total collision number was lower than 1.2 × 107. Overall, this study offers a method to apply irregular Ti and its alloys powder for AM.
engineering, chemical
What problem does this paper attempt to address?