Synthesis of silica bearing sulfobetaine and sulfonic groups and their electrorheological response

Jessica Pereira Soares,Ruan R. Henriques,Elaine Pereira,Vivian Dias,Bluma G. Soares
DOI: https://doi.org/10.1016/j.colsurfa.2023.133099
IF: 5.518
2024-01-07
Colloids and Surfaces A Physicochemical and Engineering Aspects
Abstract:Organically modified silica bearing amino groups (SiO 2 -NH 2 ) was prepared by the simple sol-gel procedure followed by treatment with butanesultone to produce zwitterionic silica bearing sulfobetaine groups (SiO 2 -SB). This particle was then treated with sulfuric acid to prepared particles carrying both sulfonic acid and ammonium salt (SiO 2 -SO 3 H). These particles were characterized by different methods and dispersed in silicone oil (15 wt%) to evaluate the electrorheological (ER) performance. Thermogravimetric (TG) analysis, zeta potential and Fourier transform infrared (FTIR) spectroscopy confirmed the structure of the modified silica. The ER response was evaluated using controlled shear stress (CSR) and oscillatory mode. The SiO 2 -NH 2 and SiO 2 -SB based fluids displayed the highest shear stress at low shear rate even without an applied electric field. However the higher ER efficiency and lower leakage current was observed for the fluid containing SiO 2 -SO 3 H. From dielectric analysis, it was demonstrated that the zwitterionic SiO 2 -SB particle provided faster relaxation time and larger permittivity difference. Thus, it is possible to conclude that the lower viscosity of the SiO 2 -SO 3 H based fluid without electric field also plays an important role for a good ER efficiency. Both SiO 2 -SB and SiO 2 -SO 3 H particles are suitable for producing ER fluids due to their better dielectric properties and relaxation time. The former also presented better sedimentation stability.
chemistry, physical
What problem does this paper attempt to address?