Effect of microstructures on mechanical properties of Ti‐6.5Al‐2Sn‐4Zr‐4Mo‐1W‐0.2Si alloy

Gang Zhou,Shewei Xin,Hui Xing,Kai Zhang,Siyuan Zhang,Zhibo Liu,Jiahao Zhang,Jian Huang,Yi Yang,Hao Wang,Aijun Huang
DOI: https://doi.org/10.1002/adem.202300012
IF: 3.6
2023-04-17
Advanced Engineering Materials
Abstract:The tensile properties at both room temperature and 550°C were investigated in Ti‐6.5Al‐2Sn‐4Zr‐4Mo‐1W‐0.2Si with three typical microstructures, which are lamellar, bimodal and equiaxed microstructures. The results show that the yield and ultimate tensile strengths decrease while the ductility increases as the volume fraction of primary α phase increasing at both temperatures. The above phenomena are resulted from the decrease in the β transformed microstructure, which is consisted by fine α and β lamellae with high density α/β interfaces blocking dislocation slipping. The yield and ultimate tensile strengths at 550°C are lower than that at room temperature, and the ductility at 550°C is higher than that at room temperature, both of which are attributed to the activity of multi slipping systems at high temperature. This article is protected by copyright. All rights reserved.
materials science, multidisciplinary
What problem does this paper attempt to address?