High Temperature Oxidation Resistance of 309S Austenitic Stainless Steel

Tang Qing-xin
Abstract:Kinetic curves of 309S at various temperatures,which were found to be parabolic,were obtained by weight gain method.Morphology of oxide scale and phase composition along depth direction were studied by SEM,XRD and XPS.The result indicated that substrates were continuously covered by oxide at different temperature.At 500 ℃,outer layer of the scale was mainly composed of Cr2O3 and Fe2O3,however,Cr2O3 and NiO were predominant phase in inner layer of the scale;at 1 000 ℃,the outer layer of the scale was mainly composed of Cr2O3,NiO,Fe3O4 or Fe2O3;while in inner layer of the scale,NiO was negligible and Cr2O3,Fe3O4 or Fe2O3 were predominant phase.