Behavior and mechanism of internal friction peak in quenched Fe-18 at.% Ga alloy

Meng Sun,Wenjie Huang,Lan Li,Weibin Jiang,Rui Gao,Wen Wen,Ting Hao,Xianping Wang,Qianfeng Fang
DOI: https://doi.org/10.1016/j.jallcom.2020.158178
IF: 6.2
2021-03-01
Journal of Alloys and Compounds
Abstract:<p>Quenched Fe-18 at.% Ga with high magnetostrictive properties has a peak (<em>P</em><sub>wq</sub>) in temperature-dependent internal friction (IF) spectrum near 320 <sup>o</sup>C, which disappears for both as-cast and furnace-cooled alloys. However, the mechanism of this peak is not well understood. In this investigation, the behavior and mechanism of this peak were systematically studied. It is found that the <em>P</em><sub>wq</sub> appears when the sample is quenched from a temperature higher than the critical temperature of the order-disorder phase transition and disappears when annealed at 300 <sup>o</sup>C for 1 h. The <em>P</em><sub>wq</sub> becomes gradually more apparent as the Ga content increases from below ~18 at.%, and the <em>P</em><sub>wq</sub> almost disappears when the Ga content equals 23 at.%. Combined with deformation and XRD studies, the <em>P</em><sub>wq</sub> does not originate from the vacancies and dislocations produced by the high-temperature quenching process or a phase transition from D0<sub>3</sub> to L1<sub>2</sub>, and potential formation mechanisms for the <em>P</em><sub>wq</sub> may originate from the transition of Ga-rich Guinier-Preston (GP) zones to D0<sub>3</sub> structures or lattice relaxation related to Ga-rich GP zones.</p>
materials science, multidisciplinary,chemistry, physical,metallurgy & metallurgical engineering
What problem does this paper attempt to address?