Role of Helium Bubbles and Voids on the Property of Nanocrystalline Tungsten

Yang Zhang,Jason Trelewicz
2024-03-19
Abstract:This manuscript embarks on an inquiry into the influence of helium implantation on nanocrystalline tungsten, a contender for plasma-facing components (PFCs) in nuclear fusion reactors. The study underscores the inevitability of helium retention in tungsten due to the anticipated high flux of helium atoms from D-T fusion reactions in future reactors such as ITER and DEMO. This retention, potentially culminating in surface blistering and grain boundary embrittlement, propels an investigation into the helium's preferential substitutional configuration over interstitial within tungsten's lattice, leading to cavity and bubble formation. Atomistic tensile testing simulations, exploiting a helium-specific interatomic potential, dissect the ramifications of helium concentration and voids on tungsten's mechanical properties across grain sizes of 10nm and 15nm. The presence of helium at grain boundaries instigates detachment, influencing structural behaviors under strain. Notably, the study reveals a dichotomy in helium's effect: benign at concentrations up to the critical point, beyond which significant embrittlement and elastic softening occur, corroborating with theoretical predictions on helium-induced grain boundary embrittlement. This nuanced exploration delineates the intricate dance between helium implantation levels, grain size, and the ensuing mechanical property alterations in nanocrystalline tungsten, casting light on its viability and endurance as a PFC material under the rigorous conditions forecasted in fusion reactors.
Materials Science,Applied Physics,Computational Physics
What problem does this paper attempt to address?
The paper attempts to address the impact of helium implantation on nanocrystalline tungsten as plasma-facing materials (PFCs) in nuclear fusion reactors. Specifically, the study focuses on the following points: 1. **Helium retention in tungsten and its effects**: Due to the high helium flux produced by D-T fusion reactions in future nuclear fusion reactors (such as ITER and DEMO), helium retention in tungsten is inevitable. This retention may lead to surface bubbling and grain boundary embrittlement. 2. **Configuration of helium in the tungsten lattice**: The study explores how helium in the tungsten lattice tends to occupy substitutional sites rather than interstitial sites, thereby forming cavities and bubbles. 3. **Impact of helium concentration and voids on mechanical properties**: Through atomic-scale tensile test simulations, the study examines the effects of different helium concentrations and voids on the mechanical properties of nanocrystalline tungsten with grain sizes of 10nm and 15nm. 4. **Helium-induced grain boundary embrittlement**: The study finds that the presence of helium at grain boundaries can lead to grain boundary separation, affecting the structural behavior of the material under strain. Notably, significant embrittlement and elastic softening occur after exceeding a critical concentration. 5. **Relationship between helium concentration and grain size**: The study reveals the complex relationship between helium concentration, grain size, and changes in the mechanical properties of the material, providing a basis for assessing the feasibility and durability of nanocrystalline tungsten in nuclear fusion reactors. Overall, through detailed simulations and analyses, the paper aims to gain an in-depth understanding of the impact of helium implantation on the mechanical properties and structural stability of nanocrystalline tungsten, providing theoretical support for its application in nuclear fusion reactors.