Characteristics of experimental hard alloy WC+(Co+Mo+Ti) in the process of friction against steels 15Kh2NMFA and 10GN2MFA without lubrication

E. V. Fominov,V. E. Gvindjiliya,R. V. Egorova,D. I. Gladckih
DOI: https://doi.org/10.1007/s11015-024-01663-z
2024-05-09
Metallurgist
Abstract:This study is dedicated to assessing the friction properties and vibration characteristics of the friction process of a hard alloy based on tungsten carbide with an experimental binder (5.65% Co + 1.8% Mo + 0.6% Ti), created based on the standard VK8 grade by partially replacing cobalt with a Mo+Ti metal group. Tribological tests were carried out without the use of a lubricant according to the "pin-on-disk" scheme during frictional interaction with steels 15Kh2NMFA and 10GN2MFA at constant load and sliding velocity. During the experiments with steel 10GN2MFA, growth of the intermediate layer in the gap between the elements of the friction pair was observed, subsequently resulting in a wider spacing between the friction bodies over time. However, no statistically significant differences were found in the gap thickness and/or roughness of the friction surfaces depending on the hard alloy grade, while the friction coefficient of the experimental composition was lower. Similarly, no significant differences in the friction surface microrelief changes on the counterbodies were found when studying the frictional interaction between samples and steel 15Kh2NMFA. However, the friction dynamics of the experimental hard alloy is characterized by lower friction coefficients and smaller thickness of the intermediate layer, as well as reduced amplitude of vibrations generated by the tribosystem dynamics itself.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?