Enhanced properties of multi‐element soluted (Nb0.8Ti0.05Zr0.05Mo0.05M0.05)4AlC3 (M = Hf, Ta) ceramics
Sumair Ahmed Soomro,Muhammad Irfan Jahanger,Maaz Ullah Khan,Yanchun Zhou,Shuai Fu,Detian Wan,Yiwang Bao,Qingguo Feng,Chunfeng Hu
DOI: https://doi.org/10.1111/ijac.14816
2024-06-14
International Journal of Applied Ceramic Technology
Abstract:(Nb0.8Ti0.05Zr0.05Mo0.05Hf0.05)4AlC3 (MAXHf) and (Nb0.8Ti0.05Zr0.05Mo0.05Ta0.05)4AlC3 (MAXTa) ceramics were successfully prepared by SPS. The XRD results confirmed the formation of a single phase of M4AlC3 hexagonal crystal structure. The EDS results showed the homogenous distribution of the elements in the samples. The EPMA results further confirmed the homogenous distribution of the atomic percentage of elements in the samples. Mechanical properties were significantly increased as compared to Nb4AlC3. The fracture toughness, flexural strength, compressive strength and Vickers hardness (10 N) of MAXHf and MAXTa ceramics were achieved as 8.87 MPa m1/2, 448 MPa, 867 MPa, 6.5 GPa and 10.36 MPa m1/2, 557 MPa, 1039 MPa, 8.2 GPa, respectively. Recently multielements solid solution has shown significant improvement to the mechanical properties of parent MAX phases. Therefore, in this work, five elements with different radii were incorporated to check the effect on properties of MAX phases. (Nb0.8Ti0.05Zr0.05Mo0.05Hf0.05)4AlC3 (MAXHf) and (Nb0.8Ti0.05Zr0.05Mo0.05Ta0.05)4AlC3 (MAXTa) ceramics were successfully synthesized using the spark plasma sintering technique. The microstructure and elemental map analysis results further confirmed that the five transition metals were successfully solid soluted at the M‐sites of the hexagonal M4AlC3 unit cell. The mean elemental compositions for M‐site elements were achieved as Nb0.85Ti0.052Zr0.035Mo0.027Hf0.036 and Nb0.847Ti0.051Zr0.043Mo0.025Ta0.033 for MAXHf and MAXTa ceramics, respectively. The electrical and thermal conductivities of multielement solid solution MAX phases were decreased compared to pure Nb4AlC3. However, Mechanical properties were significantly increased with the solid solution of five transition metals. The fracture toughness, flexural strength, compressive strength and Vickers hardness (10 N) of MAXHf and MAXTa ceramics were achieved as 8.87 MPa m1/2, 448 MPa, 867 MPa, 6.5 GPa and 10.36 MPa m1/2, 557 MPa, 1039 MPa, 8.2 GPa, respectively. The enhanced mechanical properties suggest the effectiveness of the solid solution strengthening effect and provide new opportunities to further tailor the mechanical properties of the MAX phase ceramics.
materials science, ceramics