Thulium and ytterbium-doped titanium oxide thin films deposited by ultrasonic spray pyrolysis

S. Forissier,H. Roussel,P. Chaudouet,A. Pereira,J.-L. Deschanvres,B. Moine
DOI: https://doi.org/10.1007/s11666-012-9813-7
2012-09-19
Abstract:Thin films of thulium and ytterbium-doped titanium oxide were grown by metal-organic spray pyrolysis deposition from titanium(IV)oxide bis(acetylacetonate), thulium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate) and ytterbium(III) tris(acetylacetonate). Deposition temperatures have been investigated from 300°C to 600°C. Films have been studied regarding their crystallity and doping quality. Structural and composition characterisations of TiO2:Tm,Yb were performed by electron microprobe, X-ray diffraction and Fourier transform infrared spectroscopy. The deposition rate can reach 0.8 \mum/h. The anatase phase of TiO2 was obtained after synthesis at 400°C or higher. Organic contamination at low deposition temperature is eliminated by annealing treatments.