Molecular dynamics simulation for damping properties of PDMS composite enhanced by the last generation siloxane dendrimer alcohol with hydroxyl terminal groups

Yunrui Lan,Weijin Song
DOI: https://doi.org/10.1016/j.jics.2024.101138
IF: 0.243
2024-04-01
Journal of the Indian Chemical Society
Abstract:In this study, the damping properties of PDMS composite enhanced by last generation siloxane dendrimer alcohol with hydroxyl terminal groups G3-OH were evaluated by all atomic molecular dynamics simulation (AAMDS) method in terms of damping loss factors (DLFs) tan δ , compositional miscibility ( | δ i − δ 0 | ), cohesive energy density (CED), binding energy ( E B ) and maximum free volume fraction ( F F V max ). Based on the total atomic charge distribution, further, the potential damping mechanism in composite PDMS/G3-OH(100/47) was explored. The simulation results showed that the | δ i − δ 0 | of composite PDMS/G3-OH(100/47) was 0.0939 ( J / c m 3 ) 0.5 , whose good compatibility between the two components laid a solid foundation for the excellent damping performance. As the argument, the tan δ , CED, E B and F F V max of composite PDMS/G3-OH(100/47) were 0.8073, 1.668 ( J / m 3 ) × 10 8 , −19877.607 k c a l / m o l as well as 39.85 % respectively, which were better than 1.2439, 1.390 ( J / m 3 ) × 10 8 , −14539.327 k c a l / m o l and 40.71 % of pure PDMS matrix material PDMS/G3-OH(100/0). Furthermore, the multiple hydrogen bond mechanism can perfectly explain the structure-activity relationship between the internal structure and the excellent damping properties of composite PDMS/G3-OH(100/47). Specifically, a total of 19 α-type hydrogen bonds were formed in the composite PDMS/G3-OH(100/47). All in all, according to the evaluation of AAMDS method, the PDMS composite enhanced by 47-equivalent last generation siloxane dendrimer alcohol with hydroxyl terminal groups G3-OH had outstanding damping properties.
chemistry, multidisciplinary
What problem does this paper attempt to address?