Anisotropic compressive deformation behavior of hot-rolled Mg-3Al-0.5Ce alloy

Prakash C. Gautam,Somjeet Biswas
DOI: https://doi.org/10.1016/j.jma.2024.11.015
IF: 11.813
2024-12-05
Journal of Magnesium and Alloys
Abstract:Highlights • Hot-rolled Mg-3Al-0.5Ce alloy showed anisotropic compressive behavior majorly due to basal texture. • Presence of Al 11 Ce 3 precipitates reduced the basal texture intensity, reducing the stage-II strain hardening. • Sigmoidal flow behavior ∥ to rolling (RD) & transverse direction (TD) due to extension twinning induced geometric hardening. • Parabolic flow behavior ∥ to normal direction (ND) due to slip-based deformation and no twinning. • Long-aligned Al 11 Ce 3 precipitates present within the elongated grain boundaries along RD delay the ET nucleation events. This work investigates the anisotropic compressive deformation of hot-rolled Mg-3Al-0.5Ce alloy and correlates it with microstructure and texture. Hot-rolled alloy had elongated and equiaxed grains with long-aligned Al 11 Ce 3 precipitates within the grain boundaries along rolling direction (RD) and basal texture along normal direction (ND). Analytical and crystal plasticity-based viscoplastic self-consistent predominant twin reorientation (VPSC-PTR) approaches were employed to simulate the flow curve and texture evolution for deeper insight into the deformation behavior. For compression direction (CD)∥to RD and transverse direction (TD), the basal texture was ∼⊥ to CD, which favored {101 ̄2}〈101 ̄1〉 extension twins (ET). The ETs nucleate, broaden and engulf the parent matrices with strain, rotating the lattice by ∼86.4∘ about 〈21 ̄1 ̄0〉 axes to a geometrically hard orientation with c-axis ∼∥toCD , leading to sigmoidal flow and increasing stage-II strain hardening rate (SHR). However, Al 11 Ce 3 weakened the basal texture intensity, reducing the stage-II strain hardening compared to the single-phase Mg alloy investigated earlier. The presence of Al 11 Ce 3 intermetallics delayed the ET nucleation event, which initiates at ε∼0.018 . The ET fraction evolves to ∼0.85 , lower than in the previous works on single phase Mg alloy. A reduction in the +ve SHR slope could be observed from ε = 0.03 to 0.06, indicating increased slip activities in this portion of stage-II. Beyond ε = 0.1, decreasing stage-III SHR was observed due to basal 〈 a 〉, and pyr 〈 c + a 〉- I and II slip activities in the ET orientation. The difference in the compressive behavior along RD and TD could not be observed due to Al 11 Ce 3 precipitate's morphology with elongation along RD. For CD∥to ND, the compressive flow behavior was parabolic with decreasing SHR due to slip-based deformation. ET didn't form, and the texture change was negligible, with initial and final textures having basal texture ∼∥toCD , the geometrically hard orientation. Graphical abstract Download: Download high-res image (511KB) Download: Download full-size image
metallurgy & metallurgical engineering
What problem does this paper attempt to address?