Thermoelectric Properties of an Extruded ZrO2-Modified Bi0.85Sb0.15 Solid Solution

M. M. Tagiyev,I. A. Abdullayeva,G. D. Abdinova,Kh. F. Aliyeva
DOI: https://doi.org/10.1134/s0020168523080162
2024-02-06
Inorganic Materials
Abstract:The electrical conductivity (σ), thermoelectric power (α), Hall coefficient ( R H ), and thermal conductivity (κ) of unmodified and 0.5 wt % ZrO 2 -modified extruded samples of the Bi 0.85 Sb 0.15 solid solution have been measured in the range ~77–300 K at a magnetic field strength of up to ~74 × 10 4 A/m. The results demonstrate that the addition of 0.5 wt % ZrO 2 to Bi 0.85 Sb 0.15 reduces the phonon component of its thermal conductivity, leading to an increase in its thermoelectric figure of merit ( Z ) to ~6.4 × 10 –3 K –1 . The use of the modified material is expected to considerably improve parameters of related low-temperature thermoelectric converters. At ~77 K, in both the unmodified and ZrO 2 -modified Bi 0.85 Sb 0.15 solid solutions heat is transported largely by lattice vibrations.
materials science, multidisciplinary
What problem does this paper attempt to address?