Abstract:<p>Cryptomelane-type MnO<sub>2</sub> nanomaterials with <em>a</em>-crystalline phase were prepared by heat treatment of the mixture of MnCO<sub>3</sub> and potassium oxalate followed by acid treatment. The evolution of the crystalline phase and morphology from MnCO<sub>3</sub> to cryptomelane was investigated by XRD, BET, SEM and TEM. Moreover, MnO<sub>2</sub> in nanoparticle, nanorod and nanofiber shapes could be controlled by adjusting the reaction time and temperature in the acid-treatment step. MnO<sub>2</sub> nanofibers demonstrated promoted catalytic activity and recyclability for the oxidative degradation of various organic dyes, tetracyclines and bisphenol A via peroxymonosulfate (PMS) activation. About 99% of RhB, AO7, MB, red 2 and bisphenol A at a concentration of 20–50 mg/L could be degraded over MnO<sub>2</sub> nanofibers within 12 min. Furthermore, antibiotics, like tetracycline, chlortetracycline and oxytetracycline, and bisphenol A could be mineralized efficiently, and 69–81% TOC removal was obtained. Compared to MnO<sub>2</sub> nanowires synthesized by the traditional method with KMnO<sub>4</sub>, MnO<sub>2</sub> nanofibers showed enhanced surface area (102 m<sup>2</sup>/g), more labile lattice oxygen species and higher oxygen vacancy content, which might be responsible for the superior catalytic performances. The radical quenching test and EPR analysis proved that radical (O<sub>2</sub><sup>−</sup>, SO<sub>4</sub><sup>−</sup> and OH) and non-radical (<sup>1</sup>O<sub>2</sub>) processes both existed, and the latter dominantly contributed to the degradation. Based on kinetic study, the activation energy of MnO<sub>2</sub> nanofibers/PMS for RhB degradation was only 10.55 kJ/mol, which was lower than that of MnO<sub>2</sub> nanowires (16.80 kJ/mol). This study not only offered a new, simple and economical protocol for the scaled-up synthesis of nano-scale MnO<sub>2</sub> materials, but also demonstrated its potential in water remediation.</p>
engineering, chemical