Fire resistance and burnout resistance of timber columns

Thomas Gernay
DOI: https://doi.org/10.1016/j.firesaf.2021.103350
IF: 3.78
2021-06-01
Fire Safety Journal
Abstract:<p>For any construction material, failure during or after the decay phase of a fire is possible, notably due to delayed temperature increase and material properties degradation. As mass timber construction is increasingly proposed for large buildings, there is a need to better understand the susceptibility of timber members to fire decay phases. This paper investigates the resistance to full burnout of timber columns. First, a dataset of glulam columns tested under standard fire is analyzed using finite element modeling, showing conservative agreement. Then, the numerical model is used to analyze the columns under 'standardized' natural fires comprising a cooling phase. Adopting a systematic procedure based on the minimum Duration of Heating Phase (DHP) that leads to failure, the burnout resistance of the columns is found to range from 20-50% of their standard fire resistance. These results indicate significant susceptibility to failure during the cooling phase, which is due to the combined effect of delayed heating and loss of mechanical properties at relatively low temperatures for timber. Based on heat transfer and structural mechanics, it is thus shown that guaranteeing resistance to full burnout with timber structures presents important challenges, even when setting aside the question of combustibility and auto-extinction.</p>
materials science, multidisciplinary,engineering, civil
What problem does this paper attempt to address?