Aluminum corrosion–passivation regulation prolongs aqueous batteries life

Binghang Liu,Tianshi Lv,Anxing Zhou,Xiangzhen Zhu,Zejing Lin,Ting Lin,Liumin Suo
DOI: https://doi.org/10.1038/s41467-024-47145-3
IF: 16.6
2024-04-04
Nature Communications
Abstract:Abstract Aluminum current collectors are widely used in nonaqueous batteries owing to their cost-effectiveness, lightweightness, and ease of fabrication. However, they are excluded from aqueous batteries due to their severe corrosion in aqueous solutions. Here, we propose hydrolyzation-type anodic additives to form a robust passivation layer to suppress corrosion. These additives dramatically lower the corrosion current density of aluminum by nearly three orders of magnitude to ~10 −6 A cm −2 . In addition, realizing that electrochemical corrosion accompanies anode prelithiation, we propose a prototype of self-prolonging aqueous Li-ion batteries (Al ||LiMn 2 O 4 ||TiO 2 ), whose capacity retention rises from 49.5% to 70.1% after 200 cycles. A sacrificial aluminum electrode where electrochemical corrosion is utilized is introduced as an electron supplement to prolong the cycling life of aqueous batteries. Our work addresses the short-life issue of aqueous batteries resulting from the corrosion of the current collector and lithium loss from side reactions.
multidisciplinary sciences
What problem does this paper attempt to address?