CMAS + sea salt corrosion to thermal barrier coatings

Lei Guo,Xinmu Zhang,Mingguang Liu,Shuo Yang,JianWei Dai
DOI: https://doi.org/10.1016/j.corsci.2023.111172
IF: 7.72
2023-04-14
Corrosion Science
Abstract:In marine environment, sea salt and calcium-magnesium-alumina-silicate (CMAS) coexist largely endangering thermal barrier coatings (TBCs) service safety. In this study, the corrosion behavior of synthetic sea salt and CMAS to TBCs was investigated. Sea salt changed the CMAS structure, thereby decreasing its melting temperature and high-temperature viscosity. At 1200 °C, CMAS + sea salt completely melted but CMAS did not; at 1250 °C, both melted while CMAS + sea salt had stronger penetration ability in TBCs than CMAS. Thus, TBCs which have not been or are less affected by CMAS may be damaged due to CMAS + sea salt attack.
materials science, multidisciplinary,metallurgy & metallurgical engineering