MOF-Derived CoS 2 /N-Doped Carbon Composite to Induce Short-Chain Sulfur Molecule Generation for Enhanced Sodium–Sulfur Battery Performance

Fengping Xiao,Hongkang Wang,Tianhao Yao,Xin Zhao,Xuming Yang,Denis Y. W. Yu,Andrey L. Rogach
DOI: https://doi.org/10.1021/acsami.1c02301
2021-04-06
Abstract:Dissolution of intermediate sodium polysulfides (Na<sub>2</sub>S<sub><i>x</i></sub>; 4≤<i>x</i>≤8) is a crucial obstacle for the development of room-temperature sodium-sulfur (Na–S) batteries. One promising strategy to avoid this issue is to load short-chain sulfur (S<sub>2–4</sub>), which could prohibit the generation of soluble polysulfides during the sodiation process. Herein, unlike in the previous reported cases where short-chain sulfur was stored by confinement within a small-pore-size (≤0.5 nm) carbon host, we report a new strategy to generate short-chain sulfur in larger pores (&gt;0.5 nm) by the synergistic catalytic effect of CoS<sub>2</sub> and appropriate pore size. Based on density functional theory calculations, we predict that CoS<sub>2</sub> can serve as a catalyst to weaken the S–S bond in the S<sub>8</sub> ring structure, facilitating the formation of short-chain sulfur molecules. By experimentally tuning the pore size of the CoS<sub>2</sub>-based hosts and comparing their performances as cathodes in Na–S and Li–S batteries, we conclude that such a catalytic effect depends on the proximity of sulfur to CoS<sub>2</sub>. This avoids the generation of soluble polysulfides and results in superior electrochemical properties of the composite materials introduced here for Na–S batteries. As a result, the optimized CoS<sub>2</sub>/N-doped carbon/S electrode showed excellent electrochemical performance with high reversible specific capacities of 488 mA h g<sup>–1</sup> (962 mA h g<sub>(s)</sub><sup>–1</sup>) after 100 cycles (0.1 A g<sup>–1</sup>) and 403 mA h g<sup>–1</sup> after 1000 cycles (1 A g<sup>–1</sup>) with a superior rate performance (262 mA h g<sup>–1</sup> at 5.0 A g<sup>–1</sup>).The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.1c02301?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.1c02301</a>.Structural characterization of the Co-MOF single crystals; SEM, TGA, and XPS data of the CoS<sub>2</sub>/NC and CoS<sub>2</sub>/NC/S-1-5 composites; and additional electrochemical tests for the CoS<sub>2</sub>/NC/S and LCoS<sub>2</sub>/NC/S-1-4 electrodes (<a class="ext-link" href="/doi/suppl/10.1021/acsami.1c02301/suppl_file/am1c02301_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?
This paper attempts to address the issue of sodium polysulfide (Na2Sx; 4≤x≤8) dissolution in room-temperature sodium-sulfur (Na-S) batteries. Specifically, the paper proposes a novel strategy to generate short-chain sulfur molecules (S2-4) in larger pores (>0.5 nm) through the synergistic catalytic effect of CoS2 and appropriate pore size, thereby avoiding the formation of soluble polysulfides during sodiation. This approach not only improves electrochemical performance but also avoids problems such as active sulfur loss, low coulombic efficiency, and capacity decay due to polysulfide dissolution. Key points of the paper include: 1. **Problem Background**: Room-temperature sodium-sulfur batteries have the advantages of high energy density and low cost, but the dissolution of sodium polysulfides is a major obstacle to their development. 2. **Limitations of Existing Solutions**: Previous studies have avoided the formation of sodium polysulfides by confining short-chain sulfur molecules in carbon matrices with pores smaller than 0.5 nm, but this results in low sulfur loading (about 40 wt%). 3. **New Strategy**: By generating short-chain sulfur molecules in larger pores through the synergistic catalytic effect of CoS2 and appropriate pore size, the formation of sodium polysulfides is avoided. 4. **Experimental Validation**: The effectiveness of this strategy was validated by adjusting the pore size of CoS2-based composites and using them as cathode materials for Na-S batteries. The optimized CoS2/N-doped carbon/S electrode exhibited excellent electrochemical performance, achieving a reversible specific capacity of 488 mA h g−1 (962 mA h g−1 based on sulfur mass) after 100 cycles, and maintaining a high capacity of 403 mA h g−1 after 1000 cycles. In summary, this paper presents an innovative approach to significantly improve the stability and performance of room-temperature sodium-sulfur batteries by generating short-chain sulfur molecules in larger pores through a synergistic catalytic effect.