Catalyst–Support Interaction in Polyaniline-Supported Ni3Fe Oxide to Boost Oxygen Evolution Activities for Rechargeable Zn-Air Batteries

Xiaohong Zou,Qian Lu,Mingcong Tang,Jie Wu,Kouer Zhang,Wenzhi Li,Yunxia Hu,Xiaomin Xu,Xiao Zhang,Zongping Shao,Liang An
DOI: https://doi.org/10.1007/s40820-024-01511-4
IF: 26.6
2024-09-22
Nano-Micro Letters
Abstract:Highlights Ni 3 Fe oxide, with an average size of 3.5 ± 1.5 nm, was successfully deposited onto polyaniline (PANI) support through a solvothermal strategy followed by calcination. The catalyst–support interaction between Ni 3 Fe oxide and PANI can enhance the Ni-O covalency via the interfacial Ni-N bond. Ni 3 Fe oxide/PANI-assembled Zn-air batteries achieve superior cycling life for over 400 h at 10 mA cm −2 and a low charge potential of around 1.95 V.
materials science, multidisciplinary,physics, applied,nanoscience & nanotechnology