Impact of Molding Temperature, Fiber Loading and Chemical Modifications on the Physicomechanical, and Microstructural Morphology Properties of Woven Kenaf Fiber/PLA Composites for Non-Structural Applications

Jai Inder Preet Singh,Vikas Sharma,Sehijpal Singh,Vikas Dhawan,Ahmed Belaadi,Rajeev Kumar,Shubham Sharma,Abhinav Kumar,Fuad A. Awwad,M. Ijaz Khan,Emad A. A. Ismail
DOI: https://doi.org/10.1080/15440478.2024.2326586
2024-04-29
Journal of Natural Fibers
Abstract:These days, green composites are getting a lot of attention for their biodegradability, sustainability, and affordability. This study applies polylactic acid as the matrix and untreated and surface-treated kenaf fibers as reinforcement to fabricate kenaf-reinforced PLA-based composites. Kenaf fibers are exposed to three different chemical treatments (sodium hydroxide, potassium permanganate, and potassium dichromate) and investigate the effect of surface modifications on the mechanical properties of kenaf/PLA composites. The surface modified fibers were characterized by FTIR Spectroscopy. The consequences of processing variables such as fiber volume percent ranging from 25% to 50% and molding temperature range of 160°C to 180°C were also examined on the mechanical characteristics of developed composites and are validated using SEM analysis. Surface modifications result in improved tensile and flexural characteristics of developed treated kenaf/PLA composites. Alkali treated woven kenaf fiber composites with greater matrix adhesion have optimum tensile and flexural strength of 72.81 MPa and 94.45 MPa respectively. The present study revealed that composites (fabricated at 170°C molding temperature) have maximal tensile and flexural strength at 35% fiber volume fraction. 如今,绿色复合材料因其生物降解性、可持续性和可负担性而备受关注. 本研究以聚乳酸为基体,未经处理和表面处理的红麻纤维为增强材料,制备了红麻增强聚乳酸基复合材料. 将红麻纤维暴露于三种不同的化学处理(氢氧化钠、高锰酸钾和重铬酸钾)中,研究表面改性对红麻/PLA复合材料力学性能的影响. 用红外光谱对表面改性纤维进行了表征. 还研究了加工变量(如纤维体积百分比在25%至50%范围内和成型温度在160°C至180°C范围内)对所开发复合材料的机械特性的影响,并使用SEM分析进行了验证. 表面改性改善了所开发的经处理的红麻/PLA复合材料的拉伸和弯曲特性. 基体附着力较大的碱处理红麻编织纤维复合材料的最佳拉伸强度和弯曲强度分别为72.81MPa和94.45MPa. 本研究表明,复合材料(在170°C成型温度下制造)在纤维体积分数为35%时具有最大的拉伸和弯曲强度.
materials science, textiles
What problem does this paper attempt to address?