Bisphenol A release from CAD/CAM splint materials

Tristan Hampe,Julia Liersch,Bernhard Wiechens,Ralf Bürgers,Sebastian Krohn
DOI: https://doi.org/10.1111/eos.12993
2024-05-24
European Journal Of Oral Sciences
Abstract:This study aimed to investigate the bisphenol A (BPA) release from four CAD/CAM splint materials: three polycarbonate‐based (DD BioSplint C, Splint Plus Biostar, Temp Premium Flexible) and one polymethylmethacrylate‐based (Temp Basic) material. From each material, ten cylindrical samples (n = 40) were immersed in high‐performance liquid chromatography (HPLC) grade water following ISO 10993‐12 and incubated for 24 h in an incubation shaker at 37°C and 112 rpm. Following BPA derivatization, analysis was performed by high‐performance liquid chromatography–tandem mass spectrometry (HPLC‐MS/MS). After 24 h of incubation, all investigated materials released significant amounts of BPA compared to water blanks. The material‐dependent elution increased in the following order: DD BioSplint C
dentistry, oral surgery & medicine
What problem does this paper attempt to address?