In-situ visualization of the space-charge-layer effect on interfacial lithium-ion transport in all-solid-state batteries

Longlong Wang,Ruicong Xie,Bingbing Chen,Xinrun Yu,Jun Ma,Chao Li,Zhiwei Hu,Xingwei Sun,Chengjun Xu,Shanmu Dong,Ting-Shan Chan,Jun Luo,Guanglei Cui,Liquan Chen
DOI: https://doi.org/10.1038/s41467-020-19726-5
IF: 16.6
2020-11-18
Nature Communications
Abstract:Abstract The space charge layer (SCL) is generally considered one of the origins of the sluggish interfacial lithium-ion transport in all-solid-state lithium-ion batteries (ASSLIBs). However, in-situ visualization of the SCL effect on the interfacial lithium-ion transport in sulfide-based ASSLIBs is still a great challenge. Here, we directly observe the electrode/electrolyte interface lithium-ion accumulation resulting from the SCL by investigating the net-charge-density distribution across the high-voltage LiCoO 2 /argyrodite Li 6 PS 5 Cl interface using the in-situ differential phase contrast scanning transmission electron microscopy (DPC-STEM) technique. Moreover, we further demonstrate a built-in electric field and chemical potential coupling strategy to reduce the SCL formation and boost lithium-ion transport across the electrode/electrolyte interface by the in-situ DPC-STEM technique and finite element method simulations. Our findings will strikingly advance the fundamental scientific understanding of the SCL mechanism in ASSLIBs and shed light on rational electrode/electrolyte interface design for high-rate performance ASSLIBs.
multidisciplinary sciences
What problem does this paper attempt to address?
The problem that this paper attempts to solve is: in all - solid - state lithium batteries (ASSLIBs), the hindrance of the space charge layer (SCL) to the lithium - ion transport at the electrode/electrolyte interface. Specifically, the paper aims to directly observe and understand how the SCL affects the interfacial lithium - ion transport in sulfide - based ASSLIBs through in - situ visualization techniques, and proposes a built - in electric field and chemical potential coupling strategy to reduce the formation of the SCL, thereby improving the transport efficiency of lithium ions at the electrode/electrolyte interface. ### Background of the paper All - solid - state lithium batteries (ASSLIBs) are considered as ideal substitutes for traditional liquid - electrolyte lithium batteries due to their high safety and potential high energy density. However, although sulfide solid - state electrolytes (SEs) have a relatively high room - temperature ionic conductivity (about \(10^{-2}\, \text{S/cm}\)), the performance of ASSLIBs based on these electrolytes is still inferior to that of commercial liquid - electrolyte lithium batteries, mainly because the lithium - ion transport speed at the solid - state electrode/electrolyte interface is slow. ### Influence of the space charge layer (SCL) The SCL is one of the main reasons for the slow transport of lithium ions at the solid - state electrode/electrolyte interface. The formation of the SCL will lead to the appearance of lithium - ion depletion regions (on the electrolyte side) and lithium - ion enrichment regions (on the positive electrode side) on both sides of the interface, which will significantly increase the interface resistance and become a bottleneck for lithium - ion transport. Although previous studies have attempted to study the SCL through various technical means (such as electron holographic transmission electron microscopy, spatially resolved electron energy loss spectroscopy, etc.), there has been a lack of direct experimental evidence to illustrate the specific influence of the SCL on lithium - ion transport. ### Solution To solve this problem, the authors adopted the **in - situ differential phase - contrast scanning transmission electron microscopy (DPC - STEM)** technique to directly observe the net charge density distribution at the high - voltage LiCoO₂ (LCO)/argyrodite Li₆PS₅Cl (LPSCl) interface. In addition, they also proposed a built - in electric field and chemical potential coupling strategy. By introducing ferroelectric material BaTiO₃ (BTO) nanoparticles, the formation of the SCL is suppressed, thereby accelerating the interfacial transport of lithium ions. ### Experimental results The experimental results show that in the absence of BTO coating, there are obvious lithium - ion enrichment and depletion regions at the LCO/LPSCl interface, forming a typical SCL. After coating with BTO nanoparticles, the lithium - ion distribution at the interface becomes more uniform, and the SCL effect is significantly weakened. Electrochemical performance tests also indicate that the battery coated with BTO exhibits higher capacity and better rate performance, proving the effectiveness of this strategy. ### Conclusion Through this research, the authors not only provided direct experimental evidence of the influence of the SCL on lithium - ion transport, but also proposed an effective strategy to suppress the formation of the SCL, thereby significantly improving the performance of ASSLIBs. These findings provide important scientific basis for understanding and optimizing the interface design of ASSLIBs.