Improving the signal-to-noise ratio for heat-assisted magnetic recording by optimizing a high/low Tc bilayer structure

O. Muthsam,F. Slanovc,C. Vogler,D. Suess
DOI: https://doi.org/10.1063/1.5119407
IF: 2.877
2019-09-28
Journal of Applied Physics
Abstract:We optimize the recording medium for heat-assisted magnetic recording by using a high/low <span class="equationTd inline-formula"><math> T c</math></span> bilayer structure to reduce AC and DC noise. Compared to a former work, small Gilbert damping <span class="equationTd inline-formula"><math> α = 0.02</math></span> is considered for the FePt-like hard magnetic material. Atomistic simulations are performed for a cylindrical recording grain with diameter <span class="equationTd inline-formula"><math> d = 5 nm</math></span> and height <span class="equationTd inline-formula"><math> h = 8 nm</math></span>. Different soft magnetic material compositions are tested, and the amount of hard and soft magnetic material is optimized. The results show that for a soft magnetic material with <span class="equationTd inline-formula"><math> α SM = 0.1</math></span> and <span class="equationTd inline-formula"><math> J i j , SM = 7.72 × 10 − 21 J / link</math></span>, a composition with <span class="equationTd inline-formula"><math> 50 %</math></span> hard and <span class="equationTd inline-formula"><math> 50 %</math></span> soft magnetic material leads to the best results. Additionally, we analyze how much areal density can be improved by using the optimized bilayer structure compared to the pure hard magnetic recording material. It turns out that the optimized bilayer design allows an areal density that is <span class="equationTd inline-formula"><math> 1 Tb / in . 2</math></span> higher than that of the pure hard magnetic material while obtaining the same signal-to-noise ratio.
physics, applied
What problem does this paper attempt to address?