Comparative study of continuous-stirred and batch microwave pyrolysis of linear low-density polyethylene in the presence/absence of HZSM-5

Liangliang Fan,Lei Liu,Zhiguo Xiao,Zheyang Su,Pei Huang,Hongyu Peng,Sen Lv,Haiwei Jiang,Roger Ruan,Paul Chen,Wenguang Zhou
DOI: https://doi.org/10.1016/j.energy.2021.120612
IF: 9
2021-08-01
Energy
Abstract:<p>A continuous-stirred microwave pyrolysis (CSMP) reactor was designed for linear low-density polyethylene (LLDPE) conversion. Its performance was compared with the batch microwave pyrolysis (BMP) under identical conditions. During the pyrolysis, the continuous-stirred system generated more condensate products with higher selectivity in long carbon chains (C<sub>14</sub>–C<sub>20</sub>), whereas the batch system was more selective for gas products with a higher proportion of methane. An <em>ex-situ</em> catalytic bed with HZSM-5 was assembled to upgrade pyrolysis vapors, corresponding to improved gasoline-range hydrocarbons and propylene production. The comparison of catalytic processes showed similar product yields for both configurations, with differences primarily on chemical species selectivity. For instance, the products from the continuous-stirred system had narrower carbon number distribution (C<sub>7</sub>–C<sub>10</sub>) and higher selectivity to mono-aromatics (72.3%). The proposed pathways for LLDPE conversion from the two systems showed slight differences in the thermal cracking process but similarities in the catalytic cracking process. During the catalytic processes, the potential net energy gain was 34.16 MJ/kg for CSMP and −38.86 MJ/kg for BMP, compared with the non-catalytic processes, when the figures were 9.85 MJ/kg and −42.86 MJ/kg, respectively.</p>
energy & fuels,thermodynamics
What problem does this paper attempt to address?