The influence of liquid nitrogen cooling on fracture toughness of granite rocks at elevated temperatures: An experimental study

Zuliang Shao,Xuhai Tang,Xiaoguang Wang
DOI: https://doi.org/10.1016/j.engfracmech.2021.107628
IF: 5.4
2021-04-01
Engineering Fracture Mechanics
Abstract:<p>In order to investigate the fracture toughness of granite samples after elevated temperature treatment and liquid nitrogen (LN<sub>2</sub>) cooling, a series of fracturing tests were performed on semi-circular bend (SCB) specimens containing pure mode-I fracture. The acoustic emission (AE) technique was employed to monitor the damage process during the test. The experimental results indicate that, overall, the fracture toughness of LN<sub>2</sub>-treated granite samples decreases with the increase of sample's initial temperature except at the range of 25°C to 200°C where the fracture toughness shows a slight increase with the increase of temperature. The microstructures of the granite samples after heating and LN<sub>2</sub> cooling were observed by scanning electron microscope (SEM). Isolated, short and scattered microcracks were observed within LN<sub>2</sub>-cooled granite samples with 200°C, which potentially accounts for the increased fracture toughness by blunting the pre-crack. The AE counts occur earlier for samples with higher temperature after cooling by LN<sub>2</sub>, which means the required energy for fracture initiation decreases with the increase of heating temperature. Samples with a relatively low temperature (200°C in the present study) after LN<sub>2</sub> cooling still exhibit typical brittle failure, which can be concluded by the straight drop down of loading curve and intensive release of elastic strain energy, however, a transition from brittle to ductile behavior was observed for samples with higher temperature (400°C in the present study) whose AE counts can be also monitored in the post-peak stage. Many local failure points accompanied with unique large AE counts occur on the LN<sub>2</sub>-cooled samples with higher temperature, which is the result of the connection between the pre-crack and the flaws induced by thermal stress. Besides, the fracture paths of LN<sub>2</sub>-cooled samples with lower temperature after three-point bending test will be straighter compared with those samples with higher temperature.</p>
mechanics
What problem does this paper attempt to address?