Using Laterite-Nickel Ore as Raw Material, Study on the Efficient Separation of Silicon with NaOH Alkaline Auxiliary Agent to Prepare Li2MnSiO4 Cathode for Li-ion Battery

Yuan Li,Tao Zhou,Shijie Xiong,Degang Huang
DOI: https://doi.org/10.1007/s12633-023-02805-9
IF: 3.4
2023-12-13
Silicon
Abstract:In this study, the laterite nickel ore was treated by basic hydrothermal method, and the product was dissolved directly in the form of sodium silicate. Pure SiO 2 was obtained by carbonizing sodium silicate solution. The effects of various conditions on silicon extraction rate were studied by single factor experiment. The optimum conditions of silicon leaching were as follows: NaOH concentration 75%, reaction temperature 220 °C, reaction time 110 min, liquid-solid mass ratio 4.5:1, stirring intensity 350 r/min. Orthogonal experiments were carried out to optimize the experimental parameters, and the relationship between the main and secondary factors affecting the extraction rate of silicon was determined as follows: leaching temperature > leaching time > liquid-solid mass ratio > NaOH concentration. The reaction kinetics of the mixed system was studied, and the control steps of the hydrothermal reaction process were found, that is, the process of alkali leaching of silicon from laterite nickel ore was consistent with the diffusion control law of solid product layer. Corresponding dynamic equations can be expressed as 1–3(1- α ) 2/3 + 2(1- α ) = 6.16 × exp(-8860/R T ) t . Taking SiO 2 obtained under the optimal optimization level as raw material, the Li 2 MnSiO 4 cathode material with good properties was creatively prepared by high temperature calcination method. The performance of Li 2 MnSiO 4 /C obtained by calcination at 650 °C is the best. This study provides guidance for extracting Si elements from natural minerals to prepare valuable materials.
materials science, multidisciplinary,chemistry, physical
What problem does this paper attempt to address?