A simple one-step molten salt method for synthesis of micron-sized single primary particle LiNi0.8Co0.1Mn0.1O2 cathode material for lithium-ion batteries

Rui Liang,Zhi-Yong Wu,Wen-Mao Yang,Zuo-Qin Tang,Guo-Gang Xiong,Yin-Chun Cao,Su-Rong Hu,Zhen-Bo Wang
DOI: https://doi.org/10.1007/s11581-020-03500-0
IF: 2.961
2020-02-24
Ionics
Abstract:<p class="a-plus-plus">A simple one-step molten salt method was used to synthesize micron-sized single primary particle LiNi<sub class="a-plus-plus">0.8</sub>Co<sub class="a-plus-plus">0.1</sub>Mn<sub class="a-plus-plus">0.1</sub>O<sub class="a-plus-plus">2</sub> (NCM811) cathode material. XRD, SEM, cycle performance, rate capability, differential capacity curves, 0.1 C charge/discharge curves, and EIS were carried out to research the mechanism regarding the influence of Li/transition metal (Li/TM) ratio, sinter temperature, and sinter time on the morphology and electrochemical properties of micron-sized single primary particle LiNi<sub class="a-plus-plus">0.8</sub>Co<sub class="a-plus-plus">0.1</sub>Mn<sub class="a-plus-plus">0.1</sub>O<sub class="a-plus-plus">2</sub> materials. Any one of these three factors increases exceeding certain limit and it will lead to the degradation of active structure evolution during the charge/discharge process, resulting in decreasing electrochemical performance of the cathode material. The micron-sized single primary particle NCM811 cathode material with little aggregation and primary particle size of ~ 1–2 μm was produced successfully under the condition of heating at 850 °C for 16 h with Li/TM = 1.15. This work will be helpful for the synthesis of micron-sized single primary particle NCM cathode materials for lithium-ion batteries.</p>
chemistry, physical,physics, condensed matter,electrochemistry
What problem does this paper attempt to address?