Abstract:The methylenedianiline and maleic anhydride is reacted in acetone,followed by dehydration in the presence of acetic anhydride as dehydrating agent and 1,4-diazabicyclo octane as a catalyst.Finally,the mixture of Desbimid(M-BMI) is obtained,which has a low melting point(60-80℃).The M-BMI is used in epoxy resin,whose viscosity ranges from 135-523 mPas at 80℃ as a function of the M-BMI content(0wt%-8wt%).The systems cure from 120℃ to 200℃ by step way.As a result,in contrast to unmodified epoxy resin,the flexural strength,Tg,and decomposition temperature T5% of the M-BMI-modified epoxy resin increase from 134 MPa to 154 MPa,from 139℃ to 165℃,and from 273℃to 298℃,respectively.